- Segondè dite ak dite Moh a 8 ~ 9 klas
- Segondè fwotman ak pi ba pèt fwotman
- Lajman aplikasyon pou fanm k'ap pile materyèl
- Segondè dansite ak pi fò rezistans enpak
- Rezistans chimik pou aplikasyon mwayen asid
Gwosè (mm) | D1-3 | D6/8/10/13/16/20/25 | D30/40 | D50/60 |
Tolerans (± mm) | 0.5 | 1 | 2 | 3 |
Atik | Alumina Kontni | Mohs dite | Pèt fwotman (24 èdtan) | Dansite (g/cm3) | Absòpsyon dlo |
92% boul | 92% | 9 | <0.01% | 3.6 | <0.01% |
95% boul | 95% | 9 | <0.01% | 3.74 | <0.01% |
68% boul | 68% | 7-8 | <0.03% | 3 | <0.02% |
Pwodui fason: fre-izostatik peze, oswa pa woule |
Atik | Prensipal | Dyamèt | Dansite | Sijesyon pou aplikasyon an |
(mm) | (g/cm3) | |||
CS-26 | Al2O3, SiO2 | 0.5 ~ 20 | 2.6 ~ 2.8 | Li apwopriye pou moulen an brase tankou SMD Metso a ak pwosesis fraisage amann nan materyèl mou ak dansite sispansyon ki ba. |
CS-32 | Al2O3, SiO2 ZrO2 | 0.5 ~ 20 | 3.2 ~ 3.3 | Li apwopriye pou moulen an brase tankou SMD Metso a ak fraisage mineral yo difisil. |
CS-36 | Al2O3 | 0.4 ~ 25 | 3.5 ~ 3.75 | Li apwopriye pou materyèl la Nano-gwosè fanm k'ap pile. |
CS-38 | Al2O3, ZrO2 | 0.4 ~ 20 | 3.8 ~ 3.9 | Li apwopriye pou moulen an brase tankou SMD Metso a ak fraisage mineral yo difisil. |
CS-40 | ZrO2, SiO2 | 0.4 ~ 5.0 | 4.0 ~ 4.2 | Li adapte pou fraisage gwo vitès nan minre mineral ak materyèl difisil menm jan an. |
CS-52 | ZrO2,Al2O3 | 0.4 ~ 5.0 | 5.1-5.3 | Li apwopriye pou moulen superfine materyèl la difisil ak gwo vitès (jiska 14m / S) ak opinyon enèji segondè. Pou egzanp: Moulen HIG Outotec a.Flsmidth VXP. |
CS-60 | ZrO2,Y2O3 | 0.2 ~ 40 | 5.95 ~ 6.05 | 1.Materyèl chimik, penti, enprime, lank, pigman. 2.Advanced seramik keratin oswa poud. 3.Electronic keratin: platinum lò, ajan, cuprum, nikèl. 4.Food bagay, edikaman, pwodui kosmetik. |
CS-62 | ZrO2, CeO2 | 0.6 ~ 4.0 | 6.1 ~ 6.2 |